-A A +A
Type: 
Journal
Description: 
Publisher: 
North-Holland
Publication date: 
15 Sep 2022
Authors: 

Massimo Zimbone, Maria Cantarella, Gianfranco Sfuncia, Giuseppe Nicotra, Vittorio Privitera, Enrico Napolitani, Giuliana Impellizzeri

Biblio References: 
Volume: 596 Pages: 153641
Origin: 
Applied Surface Science